Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | 9KHVG ( 9ХВГ ) |
Substitute: | ХВГ |
Classification : | Alloy tool steel |
Equivalent grades: | Go here |
C | Si | Mn | Ni | S | P | Cr | W | Cu |
0.85 - 0.95 | 0.1 - 0.4 | 0.9 - 1.2 | max 0.4 | max 0.03 | max 0.03 | 0.5 - 0.8 | 0.5 - 0.8 | max 0.3 |
Ac1 = 750 , Ac3(Acm) = 900 , Mn = 205 |
Brinell hardness for 9KHVG ( 9ХВГ ) (annealing) , GOST 5950-2000 | HB 10 -1 = 241 MPa |
USA | Germany | Japan | France | England | European | Italy | Spain | Sweden | Poland | Austria | ||||||||||||
- | DIN,WNr | JIS | AFNOR | BS | EN | UNI | UNE | SS | PN | ONORM | ||||||||||||
|
|
|
|
|
|
|
|
|
|
|
В32 - Graded and shaped rolling |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2024 Database of Steel and Alloy (russian title is the Marochnik)