Characteristics for grade     D1   ( Д1 )

      Grade :   D1   ( Д1 ) (   1110   )
      Classification :   Aluminium wrought alloys
      Equivalent grades:   Go here
Grade   D1   ( Д1 ):   supplier   Auremo   www.auremo.biz
Sale:   Russia +7 (812) 680-16-77 ,   Germany +49 (208) 205-83-073,     info [a] auremo.org



Chemical composition in % for grade   D1   ( Д1 )
Fe Si Mn Cr TiAl Cu Mg Zn Impurity -
max   0.70.2 - 0.80.4 - 1max   0.1max   0.1591.7 - 95.53.5 - 4.50.4 - 0.8max   0.25other, each 0.05; all 0.15 Ti+Zr < 0.2
Comment: Al is a basis; the percentage of Al is given approximately.


Mechanical properties under Т=20oС for grade   D1   ( Д1 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe, GOST 18482-79     335-375195-21510-12   
Bar, GOST 21488-97     195 110 12    
Bar, GOST 21488-97     355-375195-21510-12  Hardening and ageing
Bar, GOST 51834-2001     420 275 10   Hardening and ageing
Bar, GOST 51834-2001     375 215 14   Hardening and ageing
Band, GOST 13726-97     335 185 12    
Profile, GOST 18591-91     337       Hardening and ageing
Profile, GOST 8617-81     333-363186-21610-12   
Plate , GOST 17232-99     315-370195-2155-11  Hardening and ageing


    Brinell hardness for     D1   ( Д1 )   ,       HB 10 -1 = 95   MPa
    Brinell hardness for     D1   ( Д1 )   ,     annealed HB 10 -1 = 45   MPa


Physical properties for grade   D1   ( Д1 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.72     2800   54
100   22.9 130   922  


Equivalent steels for grade     D1   ( Д1 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalyPolandCzechiaAustriaSwitzerlandInter
-DIN,WNrJIS AFNORBSEN UNIPNCSNONORMSNVISO
A92017
AA2017
3.1325
AlCuMg1
2017
2017A
AU4G2017A
H14-150A
ENAW-2017A
ENAW-AlCu4MgSi(A)
AICu4MgMnSi
P-AICu4MgMn
AICuMg1
424201
AICuMg1
Al3.5Cu0.5Mg
2017
AlCu4MgSi
AlCuMgSi

Types of delivery of grade   D1   ( Д1 )
B52 - Graded and shaped rolling
B53 - Sheets and Strips
В54 - Ribbons
B55 - Bars
B64 - Pipes of non-ferrous metals and alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  D1   ( Д1 ) - Aluminium wrought alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru