Characteristics for grade     D20   ( Д20 )



      Grade :     D20   ( Д20 )
      Classification :   Aluminium wrought alloys
      Equivalent grades:     Is absent



Chemical composition in % for grade   D20   ( Д20 )
Fe Si Mn TiAl Cu Zr Mg Zn Impurity
max   0.3max   0.30.4 - 0.80.1 - 0.290.95 - 93.56 - 7max   0.2max   0.05max   0.1other, each 0.05; all 0.1
Comment: Al is a basis; the percentage of Al is given approximately.


Mechanical properties under Т=20oС for grade   D20   ( Д20 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Plate , GOST 17232-99     275   12   Guenching
Plate , GOST 17232-99     370 275 8   Quenching and artificial aging


    Brinell hardness for     D20   ( Д20 )   ,       HB 10 -1 = 100   MPa


Physical properties for grade   D20   ( Д20 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       3845    



Types of delivery of grade   D20   ( Д20 )
B52 - Graded and shaped rolling
B53 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  D20   ( Д20 ) - Aluminium wrought alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru