Grade : | V95 ( В95 ) ( 1950 ) |
Classification : | Aluminium wrought alloys |
Equivalent grades: | Go here |
Fe | Si | Mn | Ni | Cr | Ti | Al | Cu | Mg | Zn | Impurity |
max 0.5 | max 0.5 | 0.2 - 0.6 | max 0.1 | 0.1 - 0.25 | max 0.05 | 86.3 - 91.5 | 1.4 - 2 | 1.8 - 2.8 | 5 - 7 | other, each 0.05; all 0.1 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Pipe, GOST 18482-79 | 490-510 | 375-400 | 5-7 | |||||
Bar, GOST 21488-97 | 490-530 | 390-420 | 4-6 | Quenching and artificial aging | ||||
Bar, GOST 51834-2001 | 550-570 | 480-490 | 6 | Quenching and artificial aging | ||||
Band annealed , GOST 13726-97 | 245 | 10 | ||||||
Profile annealed , GOST 8617-81 | 275 | 10 | ||||||
Profile, GOST 8617-81 | 510-520 | 451-461 | 6 | |||||
Plate , GOST 17232-99 | 470-490 | 390-410 | 2-4 | Quenching and artificial aging |
Brinell hardness for V95 ( В95 ) , | HB 10 -1 = 125 MPa |
Brinell hardness for V95 ( В95 ) (quenching, ageing) , | HB 10 -1 = 150 MPa |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 0.74 | 2850 | ||||
100 | 23.2 |
USA | Germany | Japan | France | England | European | Italy | Poland | Czechia | Austria | Switzerland | Inter | ||||||||||||||||||||||
- | DIN,WNr | JIS | AFNOR | BS | EN | UNI | PN | CSN | ONORM | SNV | ISO | ||||||||||||||||||||||
|
|
|
|
|
|
|
|
|
|
|
|
B52 - Graded and shaped rolling |
B53 - Sheets and Strips |
В54 - Ribbons |
B55 - Bars |
B64 - Pipes of non-ferrous metals and alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |