Grade : | AK8M3ch ( АК8М3ч ) ( ВАЛ8 ) |
Classification : | Aluminium casting alloys |
Equivalent grades: | Is absent |
Fe | Si | Ti | Al | Cu | Zr | B | Be | Mg | Zn | Cd | Impurity |
max 0.4 | 7 - 8.5 | 0.1 - 0.25 | 85.4 - 89.65 | 2.5 - 3.5 | max 0.15 | 0.005 - 0.1 | 0.05 - 0.25 | 0.2 - 0.45 | 0.5 - 1 | max 0.15 | all 0.6 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Casting, GOST 1583-93 | 215-392 | 1-5 |
Brinell hardness for AK8M3ch ( АК8М3ч ) , Casting GOST 1583-93 | HB 10 -1 = 60 - 90 MPa |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 0.72 | 2730 | ||||
100 | 22.9 | 130 | 920 |
B51 - Non-ferrous metals, including rare metals, and their alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |