Grade : | R2M5 ( Р2М5 ) |
Classification : | High speed tool steel |
Equivalent grades: | Is absent |
C | Si | Mn | Ni | Cr | Mo | W | V | Zr |
0.95 - 1.05 | max 0.5 | max 0.5 | 0.05 - 0.08 | 3.8 - 4.3 | 4.8 - 5.3 | 1.7 - 2.3 | 0.9 - 1.3 | 0.05 - 0.15 |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |