Characteristics for grade     VCH45   ( ВЧ45 )



      Grade :     VCH45   ( ВЧ45 )
      Classification :   Cast iron with spheroidal graphite
      Equivalent grades:   Go here



Chemical composition in % for grade   VCH45   ( ВЧ45 )
C Si Mn S P Cr
2.7 - 3.80.5 - 2.90.3 - 0.7max   0.02max   0.1max   0.1


Mechanical properties under Т=20oС for grade   VCH45   ( ВЧ45 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 7293-85     450 310 10    


    Brinell hardness for     VCH45   ( ВЧ45 )   ,       GOST 7293-85 HB 10 -1 = 140 - 225   MPa


Equivalent steels for grade     VCH45   ( ВЧ45 )
Warning! Indicated both exact and nearest equivalents.
USAJapanFranceEnglandEuropeanItalyBelgiumSpainChinaBulgariaHungaryPolandAustriaAustraliaInterIndiaHollandLuxembourgCOPANT
-JIS AFNORBSEN UNINBNUNEGBBDSMSZPNONORMASISOISNEN-COPANT
65-45-12
FCD450
FGS400-12
FGS450-10
420/12
450/10
EN-GJS-450-10
EN-JS1040
GS400-12
FNG42-12
FGE42-12
QT450-10
400-12
GoV40
ZS4012
SG42
400-12
450-10
SG400/12
GN42
FNG42-12
FMNP45007



Types of delivery of grade   VCH45   ( ВЧ45 )
В81 - Castings of cast iron (gray and malleable cast iron)


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  VCH45   ( ВЧ45 ) - Cast iron with spheroidal graphite: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru