Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Structural steel

Characteristics for grade     45G   ( 45Г )

      Grade :     45G   ( 45Г )
      Substitute:   40Г, 50Г
      Classification :   Alloy structurall steel
      Equivalent grades:   Go here



Chemical composition in % for grade   45G   ( 45Г )
C Si Mn Ni S P Cr Cu
0.42 - 0.50.17 - 0.370.7 - 1max   0.3max   0.035max   0.035max   0.3max   0.3


Temperature of critical points for grade   45G   ( 45Г ).
Ac1 = 715 ,      Ac3(Acm) = 735 ,       Ar3(Arcm) = 710 ,       Ar1 = 635


Mechanical properties under Т=20oС for grade   45G   ( 45Г )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 4543-71 Ø 25   620 370 15 40490Guenching 850oC, oil, Drawing 600oC, air,


    Brinell hardness for     45G   ( 45Г )   (annealing) ,       GOST 4543-71 HB 10 -1 = 229   MPa


Technological properties for grade   45G   ( 45Г )
  Weldability: hard weldability.
Temper brittleness: weakly predisposed


Equivalent steels for grade     45G   ( 45Г )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandItalyChinaBulgariaPoland
-DIN,WNrJIS AFNORBSUNIGBBDSPN
1040
1045
1046
G10460
1.0912
46Mn7
C45E
S45C
S48C
C45E
080M46
C45
C45E
C45E
45
ML45Mn
45G
45G

Types of delivery of grade   45G   ( 45Г )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
В71 - Low-carbon steel wire


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  45G   ( 45Г ) - Alloy structurall steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru