Grade : | VT23 ( ВТ23 ) |
Classification : | Titanium wrought alloy |
Equivalent grades: | Is absent |
Fe | C | Si | Cr | Mo | V | N | Ti | Al | Zr | O | H | Impurity |
0.4 - 1 | max 0.1 | max 0.15 | 0.8 - 1.4 | 1.5 - 2.5 | 4 - 5 | max 0.05 | 84.1 - 89.3 | 4 - 6.3 | max 0.3 | max 0.15 | max 0.015 | other 0.3 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Sheet | 1100-1200 | 10-13 | Annealing | |||||
Sheet | 1450-1600 | 4-6 | Hardening and ageing |
Brinell hardness for VT23 ( ВТ23 ) (annealing) , Sheet | HB 10 -1 = 255 - 270 MPa |
Brinell hardness for VT23 ( ВТ23 ) (quenching, ageing) , Sheet | HB 10 -1 = 300 - 420 MPa |
B51 - Non-ferrous metals, including rare metals, and their alloys |
B55 - Bars |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |