Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | LK ( ЛК ) |
Classification : | Cast cooper-zinc alloys as pigs |
Equivalent grades: | Is absent |
Fe | Si | Mn | Ni | P | Al | Cu | Pb | Zn | Sb | Sn | Impurity |
max 0.6 | 2.8 - 4.5 | max 0.8 | max 0.2 | max 0.1 | max 0.1 | 76 - 81 | max 0.5 | 12 - 21.2 | max 0.1 | max 0.3 | all 2.5 |
B57 - Secondary non-ferrous metals, alloys and wastes |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)