Characteristics for grade     V2616   ( В2616 )



      Grade :     V2616   ( В2616 )
      Classification :   Aluminium casting alloys
      Equivalent grades:     Is absent



Chemical composition in % for grade   V2616   ( В2616 )
Fe Si TiAl Cu Zr B Mg Cd
max   0.46.5 - 8.50.1 - 0.386.9 - 90.692.5 - 3.50.025 - 0.050.01 - 0.10.15 - 0.40.05 - 0.3
Comment: Al is a basis; the percentage of Al is given approximately.


Mechanical properties under Т=20oС for grade   V2616   ( В2616 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
cast in a metal mould     430 370 3    
sand (mould) casting     350 300 2.5    


    Brinell hardness for     V2616   ( В2616 )   ,     cast in a metal mould HB 10 -1 = 120   MPa
    Brinell hardness for     V2616   ( В2616 )   ,     sand (mould) casting HB 10 -1 = 110   MPa


Technological properties of the material   V2616   ( В2616 ) .
        Linear shrinkage : 1.1   %


Physical properties for grade   V2616   ( В2616 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 0.72     2720    
100   22.4     880  
200   23.4        
T E 10- 5 a 10 6 l r C R 10 9




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  V2616   ( В2616 ) - Aluminium casting alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru