Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Structural steel

Characteristics for grade     45G2   ( 45Г2 )

      Grade :     45G2   ( 45Г2 )
      Substitute:   50Г2
      Classification :   Alloy structurall steel
      Equivalent grades:   Go here



Chemical composition in % for grade   45G2   ( 45Г2 )
C Si Mn Ni S P Cr Cu
0.41 - 0.490.17 - 0.371.4 - 1.8max   0.3max   0.035max   0.035max   0.3max   0.3


Temperature of critical points for grade   45G2   ( 45Г2 ).
Ac1 = 711 ,      Ac3(Acm) = 765 ,       Ar3(Arcm) = 704 ,       Ar1 = 626 ,       Mn = 245


Mechanical properties under Т=20oС for grade   45G2   ( 45Г2 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 4543-71 Ø 25   680 400 11 40 Guenching 850oC, oil, Drawing 650oC, air,


    Brinell hardness for     45G2   ( 45Г2 )   (annealing) ,       GOST 4543-71 HB 10 -1 = 229   MPa


Technological properties for grade   45G2   ( 45Г2 )
  Weldability: hard weldability.
 Flakes : weakly predisposed
Temper brittleness: predisposed


Physical properties for grade   45G2   ( 45Г2 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.04     7810    
100   11.3        
200   11.9 45   445  
300   12.7 43   428  
400     41      
500   14.7 35      
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     45G2   ( 45Г2 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanChinaSwedenBulgariaPolandAustralia
-DIN,WNrJIS GBSSBDSPNAS
1144
1345
1345H
G13450
H13450
46Mn27
SMn3
SMn433
SMn433H
45Mn2
45Mn2A
2120
45G2
45G2
X1345

Types of delivery of grade   45G2   ( 45Г2 )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  45G2   ( 45Г2 ) - Alloy structurall steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru