Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | AMK ( АМК ) |
Classification : | Alluminium antifriction alloys |
Equivalent grades: | Is absent |
Fe | Si | Mn | Ti | Al | Cu | Mg | Sb | Te | Impurity |
max 0.4 | 9 - 11 | max 0.1 | max 0.1 | 86.3 - 90.2 | 0.8 - 1.2 | max 0.3 | max 0.5 | max 0.1 | other 0.3 |
Load | Speed | Load * Speed | Temperature |
MPa | m/s | MPa * m/s | Grade |
50 | 20 | 120 |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. |