Grade : | AMg4K1.5M ( АМг4К1.5М ) ( АМг4К1.5М1 ) |
Classification : | Aluminium casting alloys |
Equivalent grades: | Is absent |
Fe | Si | Mn | Ti | Al | Cu | Be | Mg | Zn | Impurity |
max 0.4 | 1.3 - 1.7 | 0.6 - 0.9 | 0.1 - 0.25 | 90.45 - 92.8 | 0.7 - 1 | 0.002 - 0.004 | 4.5 - 5.2 | max 0.1 | all 0.3 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Casting, GOST 1583-93 | 211-265 | 2-2.3 |
Brinell hardness for AMg4K1.5M ( АМг4К1.5М ) , Casting GOST 1583-93 | HB 10 -1 = 81 - 104 MPa |
B51 - Non-ferrous metals, including rare metals, and their alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |