Characteristics for grade     V95och   ( В95оч )



      Grade :     V95och   ( В95оч )
      Classification :   Aluminium wrought alloys
      Equivalent grades:     Is absent



Chemical composition in % for grade   V95och   ( В95оч )
Fe Si Mn Cr TiAl Cu Mg Zn Impurity
max   0.15max   0.10.2 - 0.60.1 - 0.25max   0.0587.55 - 91.51.4 - 21.8 - 2.85 - 6.5other, each 0.05; all 0.1
Comment: Al is a basis; the percentage of Al is given approximately.


Physical properties for grade   V95och   ( В95оч )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       2850    




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  V95och   ( В95оч ) - Aluminium wrought alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru