Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Aluminium alloy

Characteristics for grade     V95-2   ( В95-2 )



      Grade :     V95-2   ( В95-2 )
      Classification :   Aluminium wrought alloys
      Equivalent grades:     Is absent



Chemical composition in % for grade   V95-2   ( В95-2 )
Fe Si Mn Ni CrAl Cu Mg Zn Impurity -
max   0.9max   1.50.2 - 0.8max   0.2max   0.2584.25 - 95.81 - 31 - 2.82 - 6.5other, each 0.05; all 0.2 Ti+Zr < 0.15
Comment: Al is a basis; the percentage of Al is given approximately.


Mechanical properties under Т=20oС for grade   V95-2   ( В95-2 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 21488-97     335   8-10  Hardening and ageing


Physical properties for grade   V95-2   ( В95-2 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       2850    



Types of delivery of grade   V95-2   ( В95-2 )
B53 - Sheets and Strips
B55 - Bars
B57 - Secondary non-ferrous metals, alloys and wastes


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  V95-2   ( В95-2 ) - Aluminium wrought alloys: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru