YOU HERE:   Steel and Alloy   ->   Tin

Characteristics for grade     POS61   ( ПОС61 )



      Grade :     POS61   ( ПОС61 )
      Classification :   Tin - lead solders
      Equivalent grades:     Is absent



Chemical composition in % for grade   POS61   ( ПОС61 )
Fe Ni SAl Cu As PbZn Sb Bi Sn
max   0.02max   0.02max   0.02max   0.002max   0.05max   0.0238.766 - 41max   0.002max   0.1max   0.259 - 61
Comment: Pb is a basis; the percentage of Pb is given approximately.


Mechanical properties under Т=20oС for grade   POS61   ( ПОС61 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
 , GOST 21930-76     43   46  390 


    Brinell hardness for     POS61   ( ПОС61 )   ,       GOST 21930-76 HB 10 -1 = 14   MPa


Technological properties of the material   POS61   ( ПОС61 ) .
        Melting temperature, Solidus : 183   °C
        Melting temperature, Liquidus : 190   °C


Physical properties for grade   POS61   ( ПОС61 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       8500   139



Types of delivery of grade   POS61   ( ПОС61 )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  POS61   ( ПОС61 ) - Tin - lead solders: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru