Grade : | POSSu35-2 ( ПОССу35-2 ) |
Classification : | Tin - lead solders |
Equivalent grades: | Is absent |
Fe | Ni | S | Al | Cu | As | Pb | Zn | Sb | Bi | Sn |
max 0.02 | max 0.08 | max 0.02 | max 0.002 | max 0.08 | max 0.02 | 61.776 - 64.5 | max 0.002 | 1.5 - 2 | max 0.2 | 34 - 36 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
, GOST 21930-76 | 40 | 40 | 260 |
Melting temperature, Solidus : | 185 °C |
Melting temperature, Liquidus : | 243 °C |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 9400 | 179 |
B51 - Non-ferrous metals, including rare metals, and their alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |