Characteristics for grade     30KhL   ( 30ХЛ )



      Grade :     30KhL   ( 30ХЛ )
      Classification :   Casting alloy steel for general purposes
      Equivalent grades:     Is absent



Chemical composition in % for grade   30KhL   ( 30ХЛ )
C Si Mn S P Cr
0.25 - 0.350.2 - 0.50.5 - 0.9max   0.04max   0.040.5 - 0.8


Mechanical properties under Т=20oС for grade   30KhL   ( 30ХЛ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 977-88     530 285 15 30265 
Casting, GOST 977-88     677 432 15 30402 
Casting, GOST 21357-87     660 550 10 20 Guenching and drawing


Heat treatment of the material   30KhL   ( 30ХЛ )
Normalizing 900 - 920 ° C, Tempering 550 - 650 ° C
Hardening 890 - 910° C, Tempering 620 - 660 ° C



Types of delivery of grade   30KhL   ( 30ХЛ )
B82 - Steel Castings
B83 - Castings with special properties (cast iron and steel)


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  30KhL   ( 30ХЛ ) - Casting alloy steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru