Grade : | 30HG1 ( 30ХГ1 ) ( 5МФРЛ ) |
Classification : | Casting alloy steel for general purposes |
Equivalent grades: | Is absent |
C | Si | Mn | S | P | Cr | Mo | V | B |
0.25 - 0.32 | 0.4 - 0.5 | 1.4 - 1.8 | max 0.025 | max 0.03 | 0.5 - 1 | 0.4 - 0.6 | 0.2 - 0.4 | 0.006 - 0.01 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Casting, GOST 977-88 | 981 | 638 | 4 | 5 | 49 | |||
Casting, GOST 977-88 | 1275 | 932 | 2 | 4 | 147 |
Normalizing 910 - 960 ° C |
Hardening 870 - 890 ° C, Tempering 220 - 280 ° C |
B82 - Steel Castings |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |