Characteristics for grade     A40S   ( A40S )



      Grade :     A40S   ( A40S )
      Classification :   Steel for shipbuilding
      Equivalent grades:     Is absent



Chemical composition in % for grade   A40S   ( A40S )
C Si Mn Ni S P Cr NAl Cu As
max   0.120.8 - 1.10.5 - 0.80.5 - 0.8max   0.035max   0.0350.6 - 0.9max   0.0080.015 - 0.060.4 - 0.6max   0.08


Mechanical properties under Т=20oС for grade   A40S   ( A40S )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Rolled stock, GOST 5521-93     530-690390 19    
Rolled stock, GOST 52927-2008     530-690390 20    



Types of delivery of grade   A40S   ( A40S )
В22 - Graded and shaped rolling
B23 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  A40S   ( A40S ) - Steel for shipbuilding: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru