Chemical composition in % for grade   M54   ( М54 )
C Si Mn S P As
0.45 - 0.620.15 - 0.350.5 - 0.85max   0.05max   0.04max   0.08


Mechanical properties under Т=20oС for grade   M54   ( М54 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
 , GOST 4133 - 73     844 530 10 30 Guenching


    Brinell hardness for     M54   ( М54 )   (quenching) ,       GOST 4060 HB 10 -1 = 235 - 388   MPa



Types of delivery of grade   M54   ( М54 )
B42 - Rails: Pads, Pads, Crutches


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  M54   ( М54 ) - Steel for rail transport: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru