Fe | C | Si | Mn | Ni | S | P | Cr | Ce | Mo | W | Co | Nb | Ti | Al | Zr | B | Mg |
max 0.5 | max 0.06 | max 0.5 | max 0.5 | 53.16 - 61.1 | max 0.009 | max 0.015 | 8 - 10 | max 0.01 | 2.2 - 3 | 6.5 - 7.2 | 15 - 16.5 | 1.2 - 1.6 | 1.3 - 1.7 | 4.7 - 5.2 | max 0.015 | max 0.015 | max 0.02 |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |