Characteristics for grade     VV751P   ( BB751П )



      Grade :   VV751P   ( BB751П ) (   XH56KBMTЮБ   )
      Classification :   Heat-resistant nickel alloy regranulate
      Equivalent grades:     Is absent



Chemical composition in % for grade   VV751P   ( BB751П )
Fe C Si Mn Ni S P Cr Ce Mo W V Co Nb TiAl B Pb Mg La
max   10.04 - 0.08max   0.3max   0.350.09 - 59.86max   0.009max   0.01510 - 12max   0.014 - 52.5 - 3.50.4 - 0.814 - 163 - 3.52.5 - 3.13.7 - 4.2max   0.015max   0.07max   0.01max   0.02
Comment: Ni is a basis; the percentage of Ni is given approximately.




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  VV751P   ( BB751П ) - Heat-resistant nickel alloy regranulate: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru