Characteristics for grade     38KHGN   ( 38ХГН )

      Grade :     38KHGN   ( 38ХГН )
      Substitute:   38ХГНМ
      Classification :   Alloy structurall steel
      Equivalent grades:     Is absent



Chemical composition in % for grade   38KHGN   ( 38ХГН )
C Si Mn Ni S P Cr Cu
0.35 - 0.430.17 - 0.370.8 - 1.10.7 - 1max   0.035max   0.0350.5 - 0.8max   0.3


Temperature of critical points for grade   38KHGN   ( 38ХГН ).
Ac1 = 725 ,      Ac3(Acm) = 830 ,       Ar3(Arcm) = 690 ,       Ar1 = 600 ,       Mn = 320


Mechanical properties under Т=20oС for grade   38KHGN   ( 38ХГН )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar, GOST 4543-71 Ø 25   780 685 12 45980Guenching and drawing


    Brinell hardness for     38KHGN   ( 38ХГН )   (annealing) ,       GOST 4543-71 HB 10 -1 = 229   MPa


Technological properties for grade   38KHGN   ( 38ХГН )
  Weldability: hard weldability.
 Flakes : predisposed
Temper brittleness: predisposed

Types of delivery of grade   38KHGN   ( 38ХГН )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  38KHGN   ( 38ХГН ) - Alloy structurall steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru