Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | TsA4M1v ( ЦА4М1в ) |
Classification : | Zinc casting alloys |
Equivalent grades: | Is absent |
Fe | Si | Al | Cu | Pb | Mg | Zn | Sn | Cd |
max 0.12 | max 0.03 | 3.5 - 4.5 | 0.6 - 1.3 | max 0.02 | 0.02 - 0.1 | 93.925 - 95.88 | max 0.005 | max 0.015 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
die casting, GOST 25140-93 | 196 | 0.5 |
Brinell hardness for TsA4M1v ( ЦА4М1в ) , die casting GOST 25140-93 | HB 10 -1 = 65 MPa |
B51 - Non-ferrous metals, including rare metals, and their alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)