Characteristics for grade     35N32KKhM   ( 35Н32КХМ )



      Grade :     35N32KKhM   ( 35Н32КХМ )
      Classification :   Corrosion-resistant alloy
      Equivalent grades:     Is absent



Chemical composition in % for grade   35N32KKhM   ( 35Н32КХМ )
Fe C Si Mn Ni S P Cr Mo Co Ti
max   1max   0.025max   0.15max   0.1533 - 37max   0.01max   0.01519 - 219 - 10.531 - 33max   1


Mechanical properties under Т=20oС for grade   35N32KKhM   ( 35Н32КХМ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Wire heat-treatment, GOST 51396-99     800 300 40    
Wire, GOST 51396-99     1000 650 20    
Wire cold-worked , GOST 51396-99     1200 1000 10    



Types of delivery of grade   35N32KKhM   ( 35Н32КХМ )
B73 - Steel Alloy Wire


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  35N32KKhM   ( 35Н32КХМ ) - Corrosion-resistant alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru