Characteristics for grade     30KHGSN2А   ( 30ХГСН2А )

      Grade :   30KHGSN2А   ( 30ХГСН2А ) (   30ХГСНА   )
      Classification :   Alloy structurall steel
      Equivalent grades:   Go here



Chemical composition in % for grade   30KHGSN2А   ( 30ХГСН2А )
C Si Mn Ni S P Cr Cu
0.27 - 0.340.9 - 1.21 - 1.31.4 - 1.8max   0.025max   0.0250.9 - 1.2max   0.3


Temperature of critical points for grade   30KHGSN2А   ( 30ХГСН2А ).
Ac1 = 705 ,      Ac3(Acm) = 800 ,       Mn = 321


Mechanical properties under Т=20oС for grade   30KHGSN2А   ( 30ХГСН2А )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe, GOST 21729-76     588   15    
Bar, GOST 4543-71     1620 1375 9 45590Guenching and drawing
Sheet trick, GOST 11269-76     490-830  19   Normalizing
Sheet trick, GOST 11269-76     1570   9  590Guenching and drawing
Sheet thin, GOST 11268-76     590-830  19   Normalizing
Sheet thin, GOST 11268-76     1570   9   Guenching and drawing


    Brinell hardness for     30KHGSN2А   ( 30ХГСН2А )   (annealing) ,       GOST 4543-71 HB 10 -1 = 255   MPa
    Brinell hardness for     30KHGSN2А   ( 30ХГСН2А )   (normalize) ,     Sheet trick GOST 11269-76 HB 10 -1 = 163 - 229   MPa


Technological properties for grade   30KHGSN2А   ( 30ХГСН2А )
  Weldability: hard weldability.
 Flakes : predisposed
Temper brittleness: predisposed


Physical properties for grade   30KHGSN2А   ( 30ХГСН2А )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.95   28.5 7770   440
100   10.6 29.4   0.503  
200   11.2 30.6   0.545  
300 1.8 13 31.4   0.587  
400 1.68 14.9        
500 1.35          
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     30KHGSN2А   ( 30ХГСН2А )
Warning! Indicated both exact and nearest equivalents.
BulgariaPolandCzechia
BDSPNCSN
30ChGSN2A
30HGSNA
16532

Types of delivery of grade   30KHGSN2А   ( 30ХГСН2А )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
В62 - Steel pipes and connecting parts to them


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  30KHGSN2А   ( 30ХГСН2А ) - Alloy structurall steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru