Grade : | YUNDK ( ЮНДК ) |
Classification : | Magnetically hard precision alloy |
Equivalent grades: | Is absent |
Fe | Si | Ni | Co | Ti | Al | Cu |
45.3 - 54.35 | max 1.5 | 12.5 - 15.5 | 23.5 - 25 | 0.15 - 0.5 | 7.5 - 8.7 | 2 - 3.5 |
B83 - Castings with special properties (cast iron and steel) |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |