Grade : | LS58-3 ( ЛС58-3 ) |
Classification : | Copper-zinc alloys pressure treated |
Equivalent grades: | Go here |
Fe | Ni | Al | Cu | Pb | Zn | Sn | Impurity |
max 0.5 | max 0.5 | max 0.1 | 57 - 59 | 2.5 - 3.5 | 36.3 - 40.3 | max 0.4 | all 0.2 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Bar, GOST 2060-2006 | 330 | 25 | ||||||
Bar, GOST 2060-2006 | 490 | 7 | ||||||
Bar, GOST 2060-2006 | 360 | 22 |
Brinell hardness for LS58-3 ( ЛС58-3 ) , Bar GOST 2060-2006 | HB 10 -1 = 80 MPa |
Brinell hardness for LS58-3 ( ЛС58-3 ) , Bar GOST 2060-2006 | HB 10 -1 = 130 MPa |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 8450 |
European | |
EN | |
|
B55 - Bars |
B64 - Pipes of non-ferrous metals and alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. |