Grade : | LAMsh77-2-0.04 ( ЛАМш77-2-0.04 ) |
Classification : | Copper-zinc alloys pressure treated |
Equivalent grades: | Is absent |
Fe | P | Al | Cu | As | Pb | Zn | Sb | Bi | Impurity |
max 0.1 | max 0.01 | 1.7 - 2.5 | 76 - 79 | 0.02 - 0.04 | max 0.07 | 17.98 - 21.98 | max 0.005 | max 0.002 | all 0.3 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Pipe, GOST 51573-2000 | 320 | 120 |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 8400 |
B64 - Pipes of non-ferrous metals and alloys |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |