Characteristics for grade     25Kh2N4VA   ( 25Х2Н4ВА )

      Grade :     25Kh2N4VA   ( 25Х2Н4ВА )
      Classification :   Alloy structurall steel
      Equivalent grades:     Is absent



Chemical composition in % for grade   25Kh2N4VA   ( 25Х2Н4ВА )
C Si Mn Ni S P Cr W Cu
0.21 - 0.280.17 - 0.370.25 - 0.554 - 4.4max   0.025max   0.0251.35 - 1.650.8 - 1.2max   0.3


Mechanical properties under Т=20oС for grade   25Kh2N4VA   ( 25Х2Н4ВА )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Bar Ø 25   1080 930 12 50885Guenching and drawing


    Brinell hardness for     25Kh2N4VA   ( 25Х2Н4ВА )   (annealing) ,       GOST 4543-71 HB 10 -1 = 269   MPa

Types of delivery of grade   25Kh2N4VA   ( 25Х2Н4ВА )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  25Kh2N4VA   ( 25Х2Н4ВА ) - Alloy structurall steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru