Grade : | 07Kh16N4B ( 07Х16Н4Б ) |
Classification : | Corrosion-resistant steel for general purposes |
Equivalent grades: | Is absent |
C | Si | Mn | Ni | S | P | Cr | Nb |
0.05 - 0.1 | max 0.6 | 0.2 - 0.5 | 3.5 - 4.5 | max 0.02 | max 0.025 | 15 - 16.5 | 0.2 - 0.4 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Forging, GOST 25054-81 | to 600 | longitudinal | 882 | 690 | 11-14 | 40-55 | 590-880 | Guenching and drawing |
Brinell hardness for 07Kh16N4B ( 07Х16Н4Б ) , Forging GOST 25054-81 | HB 10 -1 = 269 - 302 MPa |
B03 - Metal forming treatment. Forgings |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |