Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Structural steel

Characteristics for grade     38KH2NMF   ( 38Х2НМФ )

      Grade :     38KH2NMF   ( 38Х2НМФ )
      Substitute:   34ХН1М, 40ХН2МА, 34ХН3М
      Classification :   Alloy structurall steel
      Equivalent grades:     Is absent



Chemical composition in % for grade   38KH2NMF   ( 38Х2НМФ )
C Si Mn Ni S P Cr Mo V
0.32 - 0.420.17 - 0.370.5 - 0.80.6 - 0.9max   0.03max   0.031.8 - 2.30.2 - 0.30.08 - 0.15


Mechanical properties under Т=20oС for grade   38KH2NMF   ( 38Х2НМФ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Forging to 300   850 700 12 38500Guenching and drawing


    Brinell hardness for     38KH2NMF   ( 38Х2НМФ )   (quenching, tempering) ,       HB 10 -1 = 223 - 262   MPa


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  38KH2NMF   ( 38Х2НМФ ) - Alloy structurall steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com