Characteristics for grade     40L   ( 40Л )



      Grade :     40L   ( 40Л )
      Substitute:   45Л
      Classification :   Non-alloy casting steel
      Equivalent grades:   Go here



Chemical composition in % for grade   40L   ( 40Л )
C Si Mn S P
0.37 - 0.450.2 - 0.520.45 - 0.9max   0.06max   0.06


Temperature of critical points for grade   40L   ( 40Л ).
Ac1 = 726 ,      Ac3(Acm) = 790 ,       Ar3(Arcm) = 728 ,       Ar1 = 689


Mechanical properties under Т=20oС for grade   40L   ( 40Л )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 977-88 to 100   520 294 14 25294Normalizing 860 - 880oC,Drawing 600 - 630oC,
Casting, GOST 977-88     540 343 14 20294 


    Brinell hardness for     40L   ( 40Л )   ,       HB 10 -1 = 146 - 173   MPa


Technological properties for grade   40L   ( 40Л )
  Weldability: limited weldability.
 Flakes : not predisposed
Temper brittleness: not predisposed


Technological properties of the material   40L   ( 40Л ) .
        Linear shrinkage : 2.2 - 2.3   %


Heat treatment of the material   40L   ( 40Л )
Normalizing 860 - 880 ° C, Tempering 600 - 630 ° C
Hardening 860 - 880 ° C, Tempering 600 - 630 ° C


Physical properties for grade   40L   ( 40Л )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       7810    
100   12.4 60   470  
200   12.6 53   483  
300            
400   14.5 47   525  
500     41      
600   14.6     571  
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     40L   ( 40Л )
Warning! Indicated both exact and nearest equivalents.
USAJapanEnglandBulgariaRomaniaFinland
-JIS BSBDSSTASSFS
J04002
SCC3
CLA1gradeC
CLA8gradeC
35LI
40LI
OT550-1
G-30-57



Types of delivery of grade   40L   ( 40Л )
B42 - Rails: Pads, Pads, Crutches
B82 - Steel Castings


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  40L   ( 40Л ) - Non-alloy casting steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys