Characteristics for grade     08KH16N13M2B   ( 08Х16Н13М2Б )

      Grade :   08KH16N13M2B   ( 08Х16Н13М2Б ) (   1Х16Н13М2Б     ЭИ680   )
      Classification :   High alloy high-temperature steel
      Equivalent grades:   Go here



Chemical composition in % for grade   08KH16N13M2B   ( 08Х16Н13М2Б )
C Si Mn Ni S P Cr Mo Nb
0.06 - 0.12max   0.8max   112.5 - 14.5max   0.02max   0.03515 - 172 - 2.50.9 - 1.3


Mechanical properties under Т=20oС for grade   08KH16N13M2B   ( 08Х16Н13М2Б )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Sheet   dihedral 550 230 25  800Guenching 1000 - 1080oC, water,
Bar, GOST 5949-75   longitudinal 550 215 40 501180Guenching 1100 - 1130oC, air,


    Brinell hardness for     08KH16N13M2B   ( 08Х16Н13М2Б )   (annealing) ,     Bar GOST 5949-75 HB 10 -1 = 143 - 179   MPa


Physical properties for grade   08KH16N13M2B   ( 08Х16Н13М2Б )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 2.06     7960    
100 2   15.2      
200 1.91   17.1      
300 1.83   18.4      
400 1.74 17.1 20.1      
500 1.67 17.4 21.7      
600 1.58 17.8 23      
700   18.2 24.7      
800   18.6        
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     08KH16N13M2B   ( 08Х16Н13М2Б )
Warning! Indicated both exact and nearest equivalents.
USAGermanyFranceEnglandEuropeanItalySpainBulgariaHungaryAustria
-DIN,WNrAFNORBSEN UNIUNEBDSMSZONORM
316cd
J92971
S31640
1.4580
X1CrNiMoNb17-12-2
X6CrNiMoNb17-12-2
Z6CNDNB17-12
Z6CNDNb17-13
318S17
X6CrNiMoNb17-12-2
1.4580
X6CrNiMoNb17-12-2
X6CrNiMoNb17-2-2
X6CrNiMoNb17-12
F.3536
X6CrNiMoNb17-12-2
X6CrNiMoNb17-12-2
AoX12CrNiMoNb18-10
X6CrNiMoNb17-12-2
X6CrNiMoNb17-12-2KKW
X6CrNiMoNb17-12-2S

Types of delivery of grade   08KH16N13M2B   ( 08Х16Н13М2Б )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  08KH16N13M2B   ( 08Х16Н13М2Б ) - High alloy high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru