Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Casting steel

Characteristics for grade     30GSL   ( 30ГСЛ )



      Grade :     30GSL   ( 30ГСЛ )
      Substitute:   20ГСЛ, 25ГСЛ, 40ХЛ
      Classification :   Casting alloy steel for general purposes
      Equivalent grades:   Go here



Chemical composition in % for grade   30GSL   ( 30ГСЛ )
C Si Mn S P
0.25 - 0.350.6 - 0.81.1 - 1.4max   0.04max   0.04


Mechanical properties under Т=20oС for grade   30GSL   ( 30ГСЛ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 977-88 to 100   589 343 14 25294Normalizing 870 - 890oC,Drawing 570 - 600oC,
Casting, GOST 977-88     638 392 14 30491 


    Brinell hardness for     30GSL   ( 30ГСЛ )   ,       HB 10 -1 = 163 - 229   MPa


Technological properties for grade   30GSL   ( 30ГСЛ )
  Weldability: hard weldability.
 Flakes : not predisposed
Temper brittleness: not predisposed


Technological properties of the material   30GSL   ( 30ГСЛ ) .
        Linear shrinkage : 2.2 - 2.3   %


Heat treatment of the material   30GSL   ( 30ГСЛ )
Normalizing 870 - 890 ° C, Tempering 570 - 600 ° C
Hardening 920 - 950 ° C, Tempering 570 - 650 ° C


Equivalent steels for grade     30GSL   ( 30ГСЛ )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandBelgiumSpainChinaBulgariaHungaryRomaniaCzechiaSouth Korea
-DIN,WNrJIS AFNORBSNBNUNEGBBDSMSZSTASCSNKS
1036
1330
1330H
G13300
H13300
1.1165
30Mn5
GS-30Mn5
SCMn2
SCSiMn2
SMn433H
35M5
120M36
38Cr2
A5
A6
28Mn6
30Mn5
AM30Mn5
F.8211
F.8311
30Mn2
30G2
30GSL
Ao30MnSi5
AO35MnSi5
T30Mn14R
T30SiMn12
13141
SCMn2



Types of delivery of grade   30GSL   ( 30ГСЛ )
B82 - Steel Castings


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  30GSL   ( 30ГСЛ ) - Casting alloy steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru