Characteristics for grade     35KHMFL   ( 35ХМФЛ )



      Grade :     35KHMFL   ( 35ХМФЛ )
      Classification :   Casting alloy steel for general purposes
      Equivalent grades:     Is absent



Chemical composition in % for grade   35KHMFL   ( 35ХМФЛ )
C Si Mn Ni S P Cr Mo V Cu
0.3 - 0.40.2 - 0.40.4 - 0.9max   0.3max   0.04max   0.040.8 - 1.10.08 - 0.120.06 - 0.12max   0.3


Mechanical properties under Т=20oС for grade   35KHMFL   ( 35ХМФЛ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 21357-87 to 100   630 420 12 20340Normalizing 920oC,Drawing 640 - 700oC,
Casting, GOST 21357-87     700 550 12 25  


Technological properties of the material   35KHMFL   ( 35ХМФЛ ) .
        Linear shrinkage : 2.1   %


Heat treatment of the material   35KHMFL   ( 35ХМФЛ )
Normalizing 900 - 920 ° C, Tempering 640 - 670 ° C
Water hardening 890 - 910 ° C, Tempering 650 - 670 ° C



Types of delivery of grade   35KHMFL   ( 35ХМФЛ )
B83 - Castings with special properties (cast iron and steel)


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  35KHMFL   ( 35ХМФЛ ) - Casting alloy steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys