Characteristics for grade     03Kh18N10T   ( 03Х18Н10Т )

      Grade :   03Kh18N10T   ( 03Х18Н10Т ) (   00Х18Н10Т   )
      Classification :   High alloy high-temperature steel
      Equivalent grades:     Is absent



Chemical composition in % for grade   03Kh18N10T   ( 03Х18Н10Т )
C Si Mn Ni S P Cr -
max   0.03max   0.81 - 29.5 - 11max   0.02max   0.03517 - 18.5 (5 С - 0.4) Ti, остальное Fe


Physical properties for grade   03Kh18N10T   ( 03Х18Н10Т )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       7900    


Specification :

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  03Kh18N10T   ( 03Х18Н10Т ) - High alloy high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2018         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru