Characteristics for grade     10Kh18N10T   ( 10Х18Н10Т )



      Grade :     10Kh18N10T   ( 10Х18Н10Т )
      Classification :   Corrosion-resistant high-temperature steel
      Equivalent grades:     Is absent



Chemical composition in % for grade   10Kh18N10T   ( 10Х18Н10Т )
C Si Mn Ni S P Cr -
max   0.1max   0.81 - 210 - 11max   0.02max   0.03517 - 19 5(С - 0.02) < Ti < 0.6


Mechanical properties under Т=20oС for grade   10Kh18N10T   ( 10Х18Н10Т )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Pipe, GOST 11068-81     550 226 35    


Physical properties for grade   10Kh18N10T   ( 10Х18Н10Т )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       7900    



Types of delivery of grade   10Kh18N10T   ( 10Х18Н10Т )
В62 - Steel pipes and connecting parts to them


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  10Kh18N10T   ( 10Х18Н10Т ) - Corrosion-resistant high-temperature steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru