Chemical composition in % for grade   15GNL   ( 15ГНЛ )
C Si Mn Ni S P Cr
0.12 - 0.20.2 - 0.40.8 - 1.40.8 - 1.2max   0.03max   0.03max   0.3


Mechanical properties under Т=20oС for grade   15GNL   ( 15ГНЛ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting to 100   450 350 18 35600Normalizing 900 - 920oC,Drawing 600 - 650oC,


    Brinell hardness for     15GNL   ( 15ГНЛ )   (normalize, tempering) ,       HB 10 -1 = 140   MPa
    Brinell hardness for     15GNL   ( 15ГНЛ )   (quenching, tempering) ,       HB 10 -1 = 150   MPa


Equivalent steels for grade     15GNL   ( 15ГНЛ )
Warning! Indicated both exact and nearest equivalents.
USAGermanyFranceSpain
-DIN,WNrAFNORUNE
A350LF5
1.5622
14Ni6
16N6
15Ni6




Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  15GNL   ( 15ГНЛ ) - Casting alloy steel for general purposes: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru