Grade : | 10KH18N9L ( 10Х18Н9Л ) |
Substitute: | 14Х18Н4Г4Л |
Classification : | Casting alloy steel with specific properties |
Equivalent grades: | Go here |
C | Si | Mn | Ni | S | P | Cr |
max 0.14 | 0.2 - 1 | 1 - 2 | 8 - 11 | max 0.03 | max 0.035 | 17 - 20 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Casting, GOST 977-88 | to 100 | 441 | 177 | 25 | 35 | 981 | Guenching 1050 - 1100oC, |
Hardening 1050 - 1100 ° C, Water, oil or air cooling |
USA | Germany | Japan | France | England | Italy | China | Sweden | Bulgaria | Hungary | Poland | Romania | Czechia | South Korea | |||||||||||||||||||||||||
- | DIN,WNr | JIS | AFNOR | BS | UNI | GB | SS | BDS | MSZ | PN | STAS | CSN | KS | |||||||||||||||||||||||||
|
|
|
|
|
|
|
|
|
|
|
|
|
|
B82 - Steel Castings |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |