Characteristics for grade     12KH18N9TL   ( 12Х18Н9ТЛ )



      Grade :     12KH18N9TL   ( 12Х18Н9ТЛ )
      Classification :   Casting alloy steel with specific properties
      Equivalent grades:   Go here



Chemical composition in % for grade   12KH18N9TL   ( 12Х18Н9ТЛ )
C Si Mn Ni S P Cr Ti
max   0.120.2 - 11 - 28 - 11max   0.03max   0.03517 - 20max   0.7


Mechanical properties under Т=20oС for grade   12KH18N9TL   ( 12Х18Н9ТЛ )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Casting, GOST 977-88 to 100   441 196 25 32590Guenching 1050 - 1100oC,


Technological properties for grade   12KH18N9TL   ( 12Х18Н9ТЛ )
  Weldability: limited weldability.


Technological properties of the material   12KH18N9TL   ( 12Х18Н9ТЛ ) .
        Linear shrinkage : 2.7 - 2.8   %


Heat treatment of the material   12KH18N9TL   ( 12Х18Н9ТЛ )
Hardening 1050 - 1100 ° C, Water, oil or air cooling


Physical properties for grade   12KH18N9TL   ( 12Х18Н9ТЛ )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20 1.94   15     750
100 1.89 16.8 16   512 813
200 1.76 17 18   533 879
300 1.65 17.4 19   533 943
400 1.49 17.7 21   542 1006
500 1.38 18.1 22   554 1031
600 1.33 18.5 24   571 1082
700 1.25 18.9 25   580 1123
800 1.12 19.1 26   588 1152
900   19.1 27   596 1184
T E 10- 5 a 10 6 l r C R 10 9


Equivalent steels for grade     12KH18N9TL   ( 12Х18Н9ТЛ )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandChinaBulgariaHungaryPolandRomaniaCzechiaSouth Korea
-DIN,WNrJIS AFNORBSGBBDSMSZPNSTASCSNKS
J92630
J92701
GX10CrNi18-8
SCS13
SCS13A
Z10CN18-9M
302C25
ANC3A
ZG12Cr18Ni9Ti
ZG1Cr18Ni9
ZG1Cr18Ni9Ti
Ch18N10SL
Ch18N10TSL
AoX12CrNi18-9
AoX12CrNiTi18-9
LH18N9
LH18N9T
T15TiNiCr180
422931
422933
SSC12
SSC13A



Types of delivery of grade   12KH18N9TL   ( 12Х18Н9ТЛ )
B82 - Steel Castings


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

Weldability :
without limitations - welding is done without heating and subsequent heat treeting
limited weldability - welding is possible under heating up to 100-120 grade and subsequent heat treeting
hard weldability - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing

  12KH18N9TL   ( 12Х18Н9ТЛ ) - Casting alloy steel with specific properties: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys