Grade : | 20KH20N14S2L ( 20Х20Н14С2Л ) |
Classification : | Casting alloy steel with specific properties |
Equivalent grades: | Go here |
C | Si | Mn | Ni | S | P | Cr |
max 0.2 | 2 - 3 | max 1.5 | 12 - 15 | max 0.025 | max 0.035 | 19 - 22 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Casting, GOST 977-88 | to 100 | 491 | 245 | 20 | 25 | Normalizing 1100 - 1150oC, air, |
Weldability: | without limitations. |
Normalizing 1100 - 1150 ° C, Air cooling |
Germany | European | Poland | ||||
DIN,WNr | EN | PN | ||||
|
|
|
B82 - Steel Castings |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
Weldability : | |
without limitations | - welding is done without heating and subsequent heat treeting |
limited weldability | - welding is possible under heating up to 100-120 grade and subsequent heat treeting |
hard weldability | - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing |