Characteristics for grade     ZlSrPd585-255-160   ( ЗлСрПд585-255-160 )



      Grade :     ZlSrPd585-255-160   ( ЗлСрПд585-255-160 )
      Classification :   Gold for jewellery
      Equivalent grades:     Is absent



Chemical composition in % for grade   ZlSrPd585-255-160   ( ЗлСрПд585-255-160 )
Fe PbAg OSb Bi AuPdImpurity
max   0.15max   0.00525 - 26max   0.007max   0.005max   0.00558.5 - 5914.65 - 16.33 all 0.17
Comment: Pd is a basis; the percentage of Pd is given approximately.


Technological properties of the material   ZlSrPd585-255-160   ( ЗлСрПд585-255-160 ) .
        Melting temperature : 1175 - 1220   °C


Physical properties for grade   ZlSrPd585-255-160   ( ЗлСрПд585-255-160 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       14760    



Types of delivery of grade   ZlSrPd585-255-160   ( ЗлСрПд585-255-160 )
B53 - Sheets and Strips


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  ZlSrPd585-255-160   ( ЗлСрПд585-255-160 ) - Gold for jewellery: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru