Characteristics for grade     KH12   ( Х12 )



      Grade :     KH12   ( Х12 )
      Classification :   Die tool steel
      Equivalent grades:   Go here



Chemical composition in % for grade   KH12   ( Х12 )
C Si Mn Ni S P Cr Mo W V Ti Cu
2 - 2.20.1 - 0.40.15 - 0.45max   0.4max   0.03max   0.0311.5 - 13max   0.2max   0.2max   0.15max   0.03max   0.3


Temperature of critical points for grade   KH12   ( Х12 ).
Ac1 = 810 ,      Ac3(Acm) = 835 ,       Ar3(Arcm) = 770 ,       Ar1 = 755 ,       Mn = 180


    Brinell hardness for     KH12   ( Х12 )   (annealing) ,       GOST 5950-2000 HB 10 -1 = 255   MPa


Equivalent steels for grade     KH12   ( Х12 )
Warning! Indicated both exact and nearest equivalents.
USAGermanyJapanFranceEnglandEuropeanItalySpainChinaSwedenBulgariaPolandRomaniaCzechiaAustriaSouth Korea
-DIN,WNrJIS AFNORBSEN UNIUNEGBSSBDSPNSTASCSNONORMKS
D3
T30403
T30404
1.2060
1.2080
X210Cr12
X210CrW12
SKD1
X200CM2
X200Cr12
Z200C12
2080
BD3
1.2080
X210Cr12
X21Cr12
X205Cr12KU
F.5212
X120Cr12
X210CM2
X210Cr12
Cr12
2312
Ch12
X210Cr12
NC11
205Cr115
19436
BOHLERK100
K100
STD1



Types of delivery of grade   KH12   ( Х12 )
В32 - Graded and shaped rolling


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  KH12   ( Х12 ) - Die tool steel: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru