Characteristics for grade     ZlA-2   ( ЗлА-2 )



      Grade :     ZlA-2   ( ЗлА-2 )
      Classification :   Gold
      Equivalent grades:     Is absent



Chemical composition in % for grade   ZlA-2   ( ЗлА-2 )
FeMn Ni Cr Cu PbZn Ag Sb Bi Sn AuPtPdRhImpurity
max   0.001max   0.0005max   0.0005max   0.0005max   0.005max   0.005max   0.001max   0.015max   0.001max   0.001max   0.001min   99.98max   0.005max   0.005max   0.001 all 0.02



Types of delivery of grade   ZlA-2   ( ЗлА-2 )
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  ZlA-2   ( ЗлА-2 ) - Gold: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru