Grade : | 76Ts ( 76Ц ) |
Classification : | Steel for rail transport |
Equivalent grades: | Is absent |
C | Si | Mn | S | P | Zr |
0.71 - 0.84 | 0.18 - 0.55 | 0.75 - 1.25 | max 0.045 | max 0.035 | 0.001 - 0.01 |
Assortment | Dimension | Direct. | sв | sT | d5 | y | KCU | Heat treatment |
- | mm | - | MPa | MPa | % | % | kJ / m2 | - |
Steel, GOST 51045-97 | 780-1080 | 3-5 | 150 |
Brinell hardness for 76Ts ( 76Ц ) , Steel GOST 51045-97 | HB 10 -1 = 302 - 420 MPa |
T | E 10- 5 | a 10 6 | l | r | C | R 10 9 |
Grade | MPa | 1/Grade | Watt/(m·Grade) | kg/m3 | J/(kg·Grade) | Ohm·m |
20 | 7850 |
B42 - Rails: Pads, Pads, Crutches |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |