Characteristics for grade     Pli90-10   ( ПлИ90-10 )



      Grade :   Pli90-10   ( ПлИ90-10 ) (   ПлИ-10   )
      Classification :   Platinum alloy
      Equivalent grades:     Is absent



Chemical composition in % for grade   Pli90-10   ( ПлИ90-10 )
FePtIrImpurity -
max   0.0489.7 - 90.39.7 - 10.3 all 0.19 Pd + Rh + Au < 0.15


Mechanical properties under Т=20oС for grade   Pli90-10   ( ПлИ90-10 )
Assortment Dimension Direct. sв sT d5 y KCU Heat treatment
- mm - MPa MPa % % kJ / m2 -
Wire, GOST 18389-73 Ø 0.2 - 0.5   300-400       
Wire, GOST 18389-73 Ø 0.2 - 0.5   550-850       


Technological properties of the material   Pli90-10   ( ПлИ90-10 ) .
        Melting temperature : 1790 - 1800   °C


Physical properties for grade   Pli90-10   ( ПлИ90-10 )
T E 10- 5 a 10 6 l r C R 10 9
Grade MPa 1/Grade Watt/(m·Grade) kg/m3 J/(kg·Grade) Ohm·m
20       21540   240



Types of delivery of grade   Pli90-10   ( ПлИ90-10 )
В50 - Classification, nomenclature and general norms
B51 - Non-ferrous metals, including rare metals, and their alloys
B53 - Sheets and Strips
B74 - Wire made of non-ferrous metals and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  Pli90-10   ( ПлИ90-10 ) - Platinum alloy: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru