Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
   
YOU HERE:   Steel and Alloy   ->   Platinum, platinum alloy

Characteristics for grade     PlA-0   ( ПлА-0 )



      Grade :   PlA-0   ( ПлА-0 ) (   Пл999.8   )
      Classification :   Platinum
      Equivalent grades:     Is absent



Chemical composition in % for grade   PlA-0   ( ПлА-0 )
Fe Si Mn Ni Cr MoAl Cu As Pb Ca Mg Zn Ag Sb Bi Sn Te CdAuPtImpurity
max   0.003max   0.002max   0.005max   0.001max   0.005max   0.01max   0.002max   0.002max   0.005max   0.002max   0.005max   0.002max   0.002max   0.005max   0.001max   0.005max   0.001max   0.005max   0.005max   0.002min   99.98 all 0.02



Types of delivery of grade   PlA-0   ( ПлА-0 )
В50 - Classification, nomenclature and general norms
B51 - Non-ferrous metals, including rare metals, and their alloys


Specification :
Mechanical properties :
sв - Tensile strength , [MPa]
sT - Yield stress, [MPa]
d5 - Specific elongation at fracture , [ % ]
y - Reduction of area , [ % ]
KCU - Impact strength , [ kJ / m2]
HB - Brinell hardness , [MPa]

Physical properties :
T - Test temperature , [Grade]
E - Young modulus , [MPa]
a - Coefficient of linear expansion (range 20o - T ) , [1/Grade]
l - Termal (heat) condition coefficient , [Watt/(m·Grade)]
r - Density , [kg/m3]
C - Specific heat ( range 20o - T ), [J/(kg·Grade)]
R - Electrical resistance , [Ohm·m]

  PlA-0   ( ПлА-0 ) - Platinum: chemical composition, mechanical and physical properties, hardness
Database of steels and alloys (Marochnik) contains information about chemical composition and properties more then 3000 steels and alloys

    ©   2003 - 2025         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru